Description
ISCAR TAG N3C IC808 Insert
Family Designation: TAG N-C/W/M First choice for the parting of bars, hard materials and tough applications. A positive rake, single cavity (except 7 & 12 mm with double cavity), negative land and shoulders, provides extra cutting-edge strength. Medium-to-high feeds.
Item Designation: TAG N3C
Grade : IC808
A hard, fine grain substrate with excellent chipping resistance, combined with a new “SUMO TEC” TiAlN PVD coating. Provides high wear resistance. Recommended for a very wide range of materials.
ISO Range – P/M/K | (P15-P30)(M20-M30)(K20-K30) |
ISO Range – H/S/N | (H20-H30)(S10-S25) |
Grade or Coating Type | PVD |
Coating Layers | TiAlN/AlTiN+TiN |
Cutting Speed for: TAG N3C IC808 – 6003577
ISO | Material | Material Description | Material Condition | Cutting Speed Recommendations |
---|---|---|---|---|
P | 1 | Non-alloy steel and cast steel, free cutting steel <0.25%C | Annealed :125 | 128-188 m/min |
P | 2 | Non-alloy steel and cast steel, free cutting steel >=0.25%C | Annealed :190 | 103-158 m/min |
P | 3 | Non-alloy steel and cast steel, free cutting steel <0.55%C | Quench and tempered. :250 | 90-157 m/min |
P | 4 | Non-alloy steel and cast steel, free cutting steel >=0.55%C | Annealed :220 | 93-158 m/min |
P | 5 | Non-alloy steel and cast steel, free cutting steel >=0.55%C | Quenched & tempered. :300 | 77-147 m/min |
P | 6 | Low alloy & cast steel (less than 5% of alloying elements) | Annealed :200 | 90-143 m/min |
P | 7 | Low alloy & cast steel (less than 5% of alloying elements) | Quenched & tempered :275 | 78-138 m/min |
P | 8 | Low alloy & cast steel (less than 5% of alloying elements) | Quenched & tempered :300 | 77-134 m/min |
P | 9 | Low alloy & cast steel (less than 5% of alloying elements) | Quenched & tempered :350 | 70-120 m/min |
P | 10 | High alloyed steel, cast steel and tool steel | Annealed :200 | 93-138 m/min |
P | 11 | High alloyed steel, cast steel and tool steel | Quenched & tempered :325 | 63-110 m/min |
P | 12 | Stainless steel and cast steel | Ferritic/martensitic :200 | 90-178 m/min |
P | 13 | Stainless steel and cast steel | Martensitic :240 | 85-178 m/min |
M | 14 | Stainless steel and cast steel | Austenitic :180 | 68-152 m/min |
K | 15 | Grey cast iron (GG) | Pearlitic/ferritic :180 | 104-177 m/min |
K | 16 | Grey cast iron (GG) | Pearlitic/martensiti :260 | 90-134 m/min |
K | 17 | Nodular cast iron (GGG) | Ferritic :160 | 97-180 m/min |
K | 18 | Nodular cast iron (GGG) | Pearlitic :250 | 80-127 m/min |
K | 19 | Malleable cast iron | Ferritic :130 | 124-200 m/min |
K | 20 | Malleable cast iron | Pearlitic :230 | 100-160 m/min |
S | 31 | High temp. alloys Fe based | Annealed :200 | 28-49 m/min |
S | 32 | High temp. alloys Fe based | Cured :280 | 19-35 m/min |
S | 33 | High temp. alloys. Ni or Co based | Annealed :250 | 20-28 m/min |
S | 34 | High temp. alloys. Ni or Co based | Cured :350 | 18-24 m/min |
S | 35 | High temp. alloys. Ni or Co based | Castr :320 | 15-23 m/min |
S | 36 | Titanium (pure) | Pure :310 | 90-133 m/min |
S | 37 | Titanium Ti alloys | Alpha+beta alloys cu :310 | 30-60 m/min |
H | 38 | Hardened steel | Hardened :560 | 28-35 m/min |
H | 39 | Hardened steel | Hardened :654 | 23-33 m/min |
H | 40 | Chilled cast iron | Cast :400 | 35-53 m/min |
H | 41 | Cast iron | Hardened :560 | 30-38 m/min |