ISCAR HM390 TPKT 1003PDR IC808 Insert

​​Family Designation: HM390 TPKT 1003 Triangular inserts with 3 helical cutting edges for 90° shoulder accuracy. For general use applications

Item Designation: HM390 TPKT 1003PDR

Grade : IC808

A hard, fine grain substrate with excellent chipping resistance, combined with a new “SUMO TEC” TiAlN PVD coating. Provides high wear resistance. Recommended for a very wide range of materials. 

ISO Range – P/M/K (P15-P30)(M20-M30)(K20-K30)
ISO Range – H/S/N (H20-H30)(S10-S25)
Grade or Coating Type PVD
Coating Layers TiAlN/AlTiN+TiN

Cutting Speed for: HM390 TPKT 1003PDR IC808 – 5607513

ISO Material Material Description Material Condition Cutting Speed Recommendations
P 1 Non-alloy steel and cast steel, free cutting steel <0.25%C Annealed :125 210-300 m/min
P 2 Non-alloy steel and cast steel, free cutting steel >=0.25%C Annealed :190 200-280 m/min
P 3 Non-alloy steel and cast steel, free cutting steel <0.55%C Quench and tempered. :250 200-260 m/min
P 4 Non-alloy steel and cast steel, free cutting steel >=0.55%C Annealed :220 180-250 m/min
P 5 Non-alloy steel and cast steel, free cutting steel >=0.55%C Quenched & tempered. :300 180-240 m/min
P 6 Low alloy & cast steel (less than 5% of alloying elements) Annealed :200 170-240 m/min
P 7 Low alloy & cast steel (less than 5% of alloying elements) Quenched & tempered :275 160-230 m/min
P 8 Low alloy & cast steel (less than 5% of alloying elements) Quenched & tempered :300 150-230 m/min
P 9 Low alloy & cast steel (less than 5% of alloying elements) Quenched & tempered :350 140-220 m/min
P 10 High alloyed steel, cast steel and tool steel Annealed :200 120-210 m/min
P 11 High alloyed steel, cast steel and tool steel Quenched & tempered :325 110-170 m/min
P 12 Stainless steel and cast steel Ferritic/martensitic :200 150-230 m/min
P 13 Stainless steel and cast steel Martensitic :240 140-220 m/min
M 14 Stainless steel and cast steel Austenitic :180 100-160 m/min
S 31 High temp. alloys Fe based Annealed :200 50-60 m/min
S 32 High temp. alloys Fe based Cured :280 40-50 m/min
S 33 High temp. alloys. Ni or Co based Annealed :250 35-50 m/min
S 34 High temp. alloys. Ni or Co based Cured :350 25-35 m/min
S 35 High temp. alloys. Ni or Co based Castr :320 30-40 m/min
S 36 Titanium (pure) Pure :310 65-110 m/min
S 37 Titanium Ti alloys Alpha+beta alloys cu :310 35-70 m/min
H 38 Hardened steel Hardened :560 55-75 m/min
H 39 Hardened steel Hardened :654 45-65 m/min
H 40 Chilled cast iron Cast :400 90-105 m/min
H 41 Cast iron Hardened :560 55-75 m/min