ISCAR H490 ANKX 090408PNTR IC830 Insert

Call for Price

SKU: G-0801702 Category: Tag: Product Brands:
Sharing is caring ...

Description

ISCAR H490 ANKX 090408PNTR IC830 Insert

Family Designation: H490 ANKX/ANCX-09 Double-sided rectangular inserts with 4 helical cutting edges. Very strong construction, may be used for heavy applications. (HELIDO 490 line).

Item Designation: H490 ANKX 090408PNTR

Grade : IC830

A “SUMO TEC” TiAlN+TiN PVD coated grade. Recommended for interrupted cut and heavy operations on stainless steel, high temperature and alloyed steel. High toughness and wear resistance. 

ISO Range – P/M/K (P20-P40)(M25-M35)
ISO Range – H/S/N (S15-S30)
Grade or Coating Type PVD
Coating Layers TiAlN/AlTiN+TiN

Cutting Speed for: H490 ANKX 090408PNTR IC830 – 5606020

ISO Material Material Description Material Condition Cutting Speed Recommendations
P 1 Non-alloy steel and cast steel, free cutting steel <0.25%C Annealed :125 150-240 m/min
P 2 Non-alloy steel and cast steel, free cutting steel >=0.25%C Annealed :190 140-230 m/min
P 3 Non-alloy steel and cast steel, free cutting steel <0.55%C Quench and tempered. :250 140-230 m/min
P 4 Non-alloy steel and cast steel, free cutting steel >=0.55%C Annealed :220 130-220 m/min
P 5 Non-alloy steel and cast steel, free cutting steel >=0.55%C Quenched & tempered. :300 130-200 m/min
P 6 Low alloy & cast steel (less than 5% of alloying elements) Annealed :200 120-190 m/min
P 7 Low alloy & cast steel (less than 5% of alloying elements) Quenched & tempered :275 120-170 m/min
P 8 Low alloy & cast steel (less than 5% of alloying elements) Quenched & tempered :300 110-170 m/min
P 9 Low alloy & cast steel (less than 5% of alloying elements) Quenched & tempered :350 100-160 m/min
P 10 High alloyed steel, cast steel and tool steel Annealed :200 90-150 m/min
P 11 High alloyed steel, cast steel and tool steel Quenched & tempered :325 90-140 m/min
P 12 Stainless steel and cast steel Ferritic/martensitic :200 110-160 m/min
P 13 Stainless steel and cast steel Martensitic :240 100-150 m/min
M 14 Stainless steel and cast steel Austenitic :180 100-150 m/min
S 31 High temp. alloys Fe based Annealed :200 35-55 m/min
S 32 High temp. alloys Fe based Cured :280 30-45 m/min
S 33 High temp. alloys. Ni or Co based Annealed :250 30-45 m/min
S 34 High temp. alloys. Ni or Co based Cured :350 25-35 m/min
S 35 High temp. alloys. Ni or Co based Castr :320 30-35 m/min
S 36 Titanium (pure) Pure :310 50-90 m/min
S 37 Titanium Ti alloys Alpha+beta alloys cu :310 30-65 m/min