Description
ISCAR GTGA 16ER-IL 100 IC508 Insert
Family Designation: GTGA Precision, three cutting edges, shallow grooving inserts, used for external and internal machining
Item Designation: GTGA 16ER/IL 100
Grade : IC508
A tough submicron substrate, TiCN+TiN PVD coated grade. Designed for machining wide range of materials at low to medium cutting speeds, interrupted cut and unfavorable conditions. Excellent notch wear and built-up edge resistance.
ISO Range – P/M/K | (P20-P40)(M20-M30)(K20-K30) |
ISO Range – H/S/N | (H10-H20)(S10-S40)(N10-N30) |
Grade or Coating Type | PVD |
Coating Layers | TiCN+TiN |
Cutting Speed for: GTGA 16ER/IL 100 IC508 – 6402185
ISO | Material | Material Description | Material Condition | Cutting Speed Recommendations |
---|---|---|---|---|
P | 1 | Non-alloy steel and cast steel, free cutting steel <0.25%C | Annealed :125 | 100-150 m/min |
P | 2 | Non-alloy steel and cast steel, free cutting steel >=0.25%C | Annealed :190 | 60-100 m/min |
P | 3 | Non-alloy steel and cast steel, free cutting steel <0.55%C | Quench and tempered. :250 | 50-80 m/min |
P | 4 | Non-alloy steel and cast steel, free cutting steel >=0.55%C | Annealed :220 | 60-110 m/min |
P | 5 | Non-alloy steel and cast steel, free cutting steel >=0.55%C | Quenched & tempered. :300 | 50-80 m/min |
P | 6 | Low alloy & cast steel (less than 5% of alloying elements) | Annealed :200 | 60-110 m/min |
P | 7 | Low alloy & cast steel (less than 5% of alloying elements) | Quenched & tempered :275 | 70-110 m/min |
P | 8 | Low alloy & cast steel (less than 5% of alloying elements) | Quenched & tempered :300 | 50-80 m/min |
P | 9 | Low alloy & cast steel (less than 5% of alloying elements) | Quenched & tempered :350 | 60-90 m/min |
P | 10 | High alloyed steel, cast steel and tool steel | Annealed :200 | 60-90 m/min |
P | 11 | High alloyed steel, cast steel and tool steel | Quenched & tempered :325 | 50-80 m/min |
P | 12 | Stainless steel and cast steel | Ferritic/martensitic :200 | 50-130 m/min |
P | 13 | Stainless steel and cast steel | Martensitic :240 | 45-120 m/min |
M | 14 | Stainless steel and cast steel | Austenitic :180 | 40-130 m/min |
S | 31 | High temp. alloys Fe based | Annealed :200 | 20-40 m/min |
S | 32 | High temp. alloys Fe based | Cured :280 | 15-30 m/min |
S | 33 | High temp. alloys. Ni or Co based | Annealed :250 | 15-20 m/min |
S | 34 | High temp. alloys. Ni or Co based | Cured :350 | 15-20 m/min |
S | 35 | High temp. alloys. Ni or Co based | Castr :320 | 15-20 m/min |
S | 36 | Titanium (pure) | Pure :310 | 90-120 m/min |
S | 37 | Titanium Ti alloys | Alpha+beta alloys cu :310 | 20-50 m/min |