Description
ISCAR ECS040E05-3W06-57 IC900 Endmill 3-Fl 4mm
Family Designation: ECS/ECCS-E-3 3 flute, 38° helix short solid carbide slot / drill endmills with 3xd relieved necks and chamfered corners.
Item Designation: ECS040E05-3W06-57
Grade : IC900
A tough sub-micron PVD TiAlN coated grade. Suitable for medium to high cutting speed. Designed for machining of heat resistant alloys, austenitic stainless steel, hard alloys and carbon steel at interrupted cuts.
ISO Range – P/M/K | (P15-P30)(M20-M30)(K20-K30) |
ISO Range – H/S/N | (H20-H30)(S10-S25) |
Grade or Coating Type | PVD |
Coating Layers | TiAlN |
Cutting Speed for: ECS040E05-3W06-57 IC900 – 5620549
ISO | Material | Material Description | Material Condition | Cutting Speed Recommendations |
---|---|---|---|---|
P | 1 | Non-alloy steel and cast steel, free cutting steel <0.25%C | Annealed :125 | 250-270 m/min |
P | 2 | Non-alloy steel and cast steel, free cutting steel >=0.25%C | Annealed :190 | 200-230 m/min |
P | 3 | Non-alloy steel and cast steel, free cutting steel <0.55%C | Quench and tempered. :250 | 160-220 m/min |
P | 4 | Non-alloy steel and cast steel, free cutting steel >=0.55%C | Annealed :220 | 160-220 m/min |
P | 5 | Non-alloy steel and cast steel, free cutting steel >=0.55%C | Quenched & tempered. :300 | 140-180 m/min |
P | 6 | Low alloy & cast steel (less than 5% of alloying elements) | Annealed :200 | 160-220 m/min |
P | 7 | Low alloy & cast steel (less than 5% of alloying elements) | Quenched & tempered :275 | 120-180 m/min |
P | 8 | Low alloy & cast steel (less than 5% of alloying elements) | Quenched & tempered :300 | 130-180 m/min |
P | 9 | Low alloy & cast steel (less than 5% of alloying elements) | Quenched & tempered :350 | 140-180 m/min |
P | 10 | High alloyed steel, cast steel and tool steel | Annealed :200 | 130-180 m/min |
P | 11 | High alloyed steel, cast steel and tool steel | Quenched & tempered :325 | 70-120 m/min |
P | 12 | Stainless steel and cast steel | Ferritic/martensitic :200 | 80-160 m/min |
P | 13 | Stainless steel and cast steel | Martensitic :240 | 60-150 m/min |
M | 14 | Stainless steel and cast steel | Austenitic :180 | 60-120 m/min |
K | 15 | Grey cast iron (GG) | Pearlitic/ferritic :180 | 80-250 m/min |
K | 16 | Grey cast iron (GG) | Pearlitic/martensiti :260 | 130-240 m/min |
K | 17 | Nodular cast iron (GGG) | Ferritic :160 | 150-270 m/min |
K | 18 | Nodular cast iron (GGG) | Pearlitic :250 | 150-270 m/min |
K | 19 | Malleable cast iron | Ferritic :130 | 150-270 m/min |
K | 20 | Malleable cast iron | Pearlitic :230 | 140-240 m/min |
S | 31 | High temp. alloys Fe based | Annealed :200 | 20-40 m/min |
S | 32 | High temp. alloys Fe based | Cured :280 | 20-30 m/min |
S | 33 | High temp. alloys. Ni or Co based | Annealed :250 | 20-30 m/min |
S | 34 | High temp. alloys. Ni or Co based | Cured :350 | 20-30 m/min |
S | 35 | High temp. alloys. Ni or Co based | Castr :320 | 20-30 m/min |
S | 36 | Titanium (pure) | Pure :310 | 30-80 m/min |
S | 37 | Titanium Ti alloys | Alpha+beta alloys cu :310 | 30-80 m/min |