Deskripsi
ISCAR EC040 B12-4C06 IC900 Endmill
ISCAR EC040 B12-4C06 IC900 Endmill. A tough sub-micron PVD TiAlN coated grade. Suitable for medium to high cutting speed. Designed for machining of heat resistant alloys, austenitic stainless steel, hard alloys and carbon steel at interrupted cuts.
| ISO Range – P/M/K |
(P15-P30)(M20-M30)(K20-K30) |
| ISO Range – H/S/N |
(H20-H30)(S10-S25) |
| Grade or Coating Type |
PVD |
| Coating Layers |
TiAlN |
Cutting Speed for: EC040B12-4C06 IC900 – 5620729
| SO |
Material |
Material Description |
Material Condition |
Cutting Speed Recommendations |
| P |
1 |
Non-alloy steel and cast steel, free cutting steel <0.25%C |
Annealed :125 |
250-270 m/min |
| P |
2 |
Non-alloy steel and cast steel, free cutting steel >=0.25%C |
Annealed :190 |
200-230 m/min |
| P |
3 |
Non-alloy steel and cast steel, free cutting steel <0.55%C |
Quench and tempered. :250 |
160-220 m/min |
| P |
4 |
Non-alloy steel and cast steel, free cutting steel >=0.55%C |
Annealed :220 |
160-220 m/min |
| P |
5 |
Non-alloy steel and cast steel, free cutting steel >=0.55%C |
Quenched & tempered. :300 |
140-180 m/min |
| P |
6 |
Low alloy & cast steel (less than 5% of alloying elements) |
Annealed :200 |
160-220 m/min |
| P |
7 |
Low alloy & cast steel (less than 5% of alloying elements) |
Quenched & tempered :275 |
120-180 m/min |
| P |
8 |
Low alloy & cast steel (less than 5% of alloying elements) |
Quenched & tempered :300 |
130-180 m/min |
| P |
9 |
Low alloy & cast steel (less than 5% of alloying elements) |
Quenched & tempered :350 |
140-180 m/min |
| P |
10 |
High alloyed steel, cast steel and tool steel |
Annealed :200 |
130-180 m/min |
| P |
11 |
High alloyed steel, cast steel and tool steel |
Quenched & tempered :325 |
70-120 m/min |
| P |
12 |
Stainless steel and cast steel |
Ferritic/martensitic :200 |
80-160 m/min |
| P |
13 |
Stainless steel and cast steel |
Martensitic :240 |
60-150 m/min |
| M |
14 |
Stainless steel and cast steel |
Austenitic :180 |
60-120 m/min |
| K |
15 |
Grey cast iron (GG) |
Pearlitic/ferritic :180 |
80-250 m/min |
| K |
16 |
Grey cast iron (GG) |
Pearlitic/martensiti :260 |
130-240 m/min |
| K |
17 |
Nodular cast iron (GGG) |
Ferritic :160 |
150-270 m/min |
| K |
18 |
Nodular cast iron (GGG) |
Pearlitic :250 |
150-270 m/min |
| K |
19 |
Malleable cast iron |
Ferritic :130 |
150-270 m/min |
| K |
20 |
Malleable cast iron |
Pearlitic :230 |
140-240 m/min |
| S |
31 |
High temp. alloys Fe based |
Annealed :200 |
20-40 m/min |
| S |
32 |
High temp. alloys Fe based |
Cured :280 |
20-30 m/min |
| S |
33 |
High temp. alloys. Ni or Co based |
Annealed :250 |
20-30 m/min |
| S |
34 |
High temp. alloys. Ni or Co based |
Cured :350 |
20-30 m/min |
| S |
35 |
High temp. alloys. Ni or Co based |
Castr :320 |
20-30 m/min |
| S |
36 |
Titanium (pure) |
Pure :310 |
30-80 m/min |
| S |
37 |
Titanium Ti alloys |
Alpha+beta alloys cu :310 |
30-80 m/min |
| H |
38 |
Hardened steel |
Hardened :560 |
30-60 m/min |
| H |
39 |
Hardened steel |
Hardened :654 |
30-40 m/min |
| H |
40 |
Chilled cast iron |
Cast :400 |
70-90 m/min |
| H |
41 |
Cast iron |
Hardened :560 |
30-60 m/min |