ISCAR EC-A2 200-38C20-105 IC903 Endmill

Family Designation: EC-A2 (medium length) 2 flute, 30° helix medium length solid carbide endmills for hard materials up to 65 HRC.

Item Designation: EC-A2 200-38C20-105

Grade : IC903

Ultra-fine carbide grain with 12% cobalt, TiAlN PV D coated. High wear resistance and toughness. High speed, medium feed. Used for up to 62Rc hardened steel, titanium, nickel-based alloys and stainless steel. 

ISO Range – P/M/K (P10-P20)(M15-M25)(K10-K20)
ISO Range – H/S/N (H10-H20)(S10-S20)
Grade or Coating Type PVD
Coating Layers TiAlN

Cutting Speed for: EC-A2 200-38C20-105 IC903 – 5650914

ISO Material Material Description Material Condition Cutting Speed Recommendations
P 1 Non-alloy steel and cast steel, free cutting steel <0.25%C Annealed :125 250-270 m/min
P 2 Non-alloy steel and cast steel, free cutting steel >=0.25%C Annealed :190 200-230 m/min
P 3 Non-alloy steel and cast steel, free cutting steel <0.55%C Quench and tempered. :250 160-220 m/min
P 4 Non-alloy steel and cast steel, free cutting steel >=0.55%C Annealed :220 160-220 m/min
P 5 Non-alloy steel and cast steel, free cutting steel >=0.55%C Quenched & tempered. :300 140-180 m/min
P 6 Low alloy & cast steel (less than 5% of alloying elements) Annealed :200 160-220 m/min
P 7 Low alloy & cast steel (less than 5% of alloying elements) Quenched & tempered :275 120-180 m/min
P 8 Low alloy & cast steel (less than 5% of alloying elements) Quenched & tempered :300 130-180 m/min
P 9 Low alloy & cast steel (less than 5% of alloying elements) Quenched & tempered :350 140-180 m/min
P 10 High alloyed steel, cast steel and tool steel Annealed :200 130-180 m/min
P 11 High alloyed steel, cast steel and tool steel Quenched & tempered :325 70-120 m/min
P 12 Stainless steel and cast steel Ferritic/martensitic :200 80-160 m/min
P 13 Stainless steel and cast steel Martensitic :240 60-150 m/min
M 14 Stainless steel and cast steel Austenitic :180 60-120 m/min
K 15 Grey cast iron (GG) Pearlitic/ferritic :180 80-250 m/min
K 16 Grey cast iron (GG) Pearlitic/martensiti :260 130-240 m/min
K 17 Nodular cast iron (GGG) Ferritic :160 150-270 m/min
K 18 Nodular cast iron (GGG) Pearlitic :250 90-270 m/min
K 19 Malleable cast iron Ferritic :130 150-270 m/min
K 20 Malleable cast iron Pearlitic :230 140-240 m/min
S 31 High temp. alloys Fe based Annealed :200 20-40 m/min
S 32 High temp. alloys Fe based Cured :280 20-30 m/min
S 33 High temp. alloys. Ni or Co based Annealed :250 20-30 m/min
S 34 High temp. alloys. Ni or Co based Cured :350 20-30 m/min
S 35 High temp. alloys. Ni or Co based Castr :320 30-80 m/min
S 36 Titanium (pure) Pure :310 30-80 m/min
S 37 Titanium Ti alloys Alpha+beta alloys cu :310 30-80 m/min
H 38 Hardened steel Hardened :560 30-60 m/min
H 39 Hardened steel Hardened :654 30-40 m/min
H 40 Chilled cast iron Cast :400 70-90 m/min
H 41 Cast iron Hardened :560 30-60 m/min