ISCAR DGN 2502C IC908 Insert

Family Designation: DGN/DGNC/DGNM-C Used for parting bars, hard materials and tough applications. A positive rake, single cavity with a negative land and shoulders. Medium-to-high feeds. DGNC – with coolant holes, DGNM – single ended for very deep applications.

Item Designation: DGN 2502C

Grade : IC908

A hard, fine grain substrate with excellent chippi ng resistance, combined with a TiAlN PVD coating. Provides high wear and oxidation resistance. Recom mended for a very wide range of materials applicat ions and machining conditions. 

ISO Range – P/M/K (P15-P30)(M20-M30)(K20-K30)
ISO Range – H/S/N (H20-H30)(S10-S25)
Grade or Coating Type PVD
Coating Layers TiAlN

Cutting Speed for: DGN 2502C IC908 – 6003489

ISO Material Material Description Material Condition Cutting Speed Recommendations
P 1 Non-alloy steel and cast steel, free cutting steel <0.25%C Annealed :125 120-183 m/min
P 2 Non-alloy steel and cast steel, free cutting steel >=0.25%C Annealed :190 90-145 m/min
P 3 Non-alloy steel and cast steel, free cutting steel <0.55%C Quench and tempered. :250 73-123 m/min
P 4 Non-alloy steel and cast steel, free cutting steel >=0.55%C Annealed :220 83-148 m/min
P 5 Non-alloy steel and cast steel, free cutting steel >=0.55%C Quenched & tempered. :300 65-118 m/min
P 6 Low alloy & cast steel (less than 5% of alloying elements) Annealed :200 80-133 m/min
P 7 Low alloy & cast steel (less than 5% of alloying elements) Quenched & tempered :275 78-133 m/min
P 8 Low alloy & cast steel (less than 5% of alloying elements) Quenched & tempered :300 65-110 m/min
P 9 Low alloy & cast steel (less than 5% of alloying elements) Quenched & tempered :350 70-115 m/min
P 10 High alloyed steel, cast steel and tool steel Annealed :200 80-123 m/min
P 11 High alloyed steel, cast steel and tool steel Quenched & tempered :325 60-103 m/min
P 12 Stainless steel and cast steel Ferritic/martensitic :200 70-160 m/min
P 13 Stainless steel and cast steel Martensitic :240 63-148 m/min
M 14 Stainless steel and cast steel Austenitic :180 55-140 m/min
K 15 Grey cast iron (GG) Pearlitic/ferritic :180 105-185 m/min
K 16 Grey cast iron (GG) Pearlitic/martensiti :260 100-145 m/min
K 17 Nodular cast iron (GGG) Ferritic :160 110-200 m/min
K 18 Nodular cast iron (GGG) Pearlitic :250 90-135 m/min
K 19 Malleable cast iron Ferritic :130 130-215 m/min
K 20 Malleable cast iron Pearlitic :230 110-170 m/min
S 31 High temp. alloys Fe based Annealed :200 28-48 m/min
S 32 High temp. alloys Fe based Cured :280 19-34 m/min
S 33 High temp. alloys. Ni or Co based Annealed :250 19-27 m/min
S 34 High temp. alloys. Ni or Co based Cured :350 18-24 m/min
S 35 High temp. alloys. Ni or Co based Castr :320 18-23 m/min
S 36 Titanium (pure) Pure :310 90-130 m/min
S 37 Titanium Ti alloys Alpha+beta alloys cu :310 29-59 m/min
H 38 Hardened steel Hardened :560 25-35 m/min
H 39 Hardened steel Hardened :654 23-33 m/min
H 40 Chilled cast iron Cast :400 28-43 m/min
H 41 Cast iron Hardened :560 28-38 m/min