ISCAR ECR-B4M 05-10W06-57 IC900 Endmill

Call for Price

Sharing is caring ...

Deskripsi

ISCAR ECR-B4M 05-10W06-57 IC900 Endmill

Family Designation: ECR-B-M/ECR-B-M…R 4-7 flute, 45° helix medium length (2xd) solid carbide roughing endmills. Used for high stock removal rates.

Item Designation: ECR-B4M 05-10W06-57

Grade : IC900

A tough sub-micron PVD TiAlN coated grade. Suitable for medium to high cutting speed. Designed for machining of heat resistant alloys, austenitic stainless steel, hard alloys and carbon steel at interrupted cuts. 

ISO Range – P/M/K (P15-P30)(M20-M30)(K20-K30)
ISO Range – H/S/N (H20-H30)(S10-S25)
Grade or Coating Type PVD
Coating Layers TiAlN

Cutting Speed for: ECR-B4M 05-10W06-57 IC900 – 5621508

ISO Material Material Description Material Condition Cutting Speed Recommendations
P 1 Non-alloy steel and cast steel, free cutting steel <0.25%C Annealed :125 250-270 m/min
P 2 Non-alloy steel and cast steel, free cutting steel >=0.25%C Annealed :190 200-230 m/min
P 3 Non-alloy steel and cast steel, free cutting steel <0.55%C Quench and tempered. :250 160-220 m/min
P 4 Non-alloy steel and cast steel, free cutting steel >=0.55%C Annealed :220 160-220 m/min
P 5 Non-alloy steel and cast steel, free cutting steel >=0.55%C Quenched & tempered. :300 140-180 m/min
P 6 Low alloy & cast steel (less than 5% of alloying elements) Annealed :200 160-220 m/min
P 7 Low alloy & cast steel (less than 5% of alloying elements) Quenched & tempered :275 120-180 m/min
P 8 Low alloy & cast steel (less than 5% of alloying elements) Quenched & tempered :300 130-180 m/min
P 9 Low alloy & cast steel (less than 5% of alloying elements) Quenched & tempered :350 140-180 m/min
P 10 High alloyed steel, cast steel and tool steel Annealed :200 130-180 m/min
P 11 High alloyed steel, cast steel and tool steel Quenched & tempered :325 70-120 m/min
P 12 Stainless steel and cast steel Ferritic/martensitic :200 80-160 m/min
P 13 Stainless steel and cast steel Martensitic :240 60-150 m/min
M 14 Stainless steel and cast steel Austenitic :180 60-120 m/min
K 15 Grey cast iron (GG) Pearlitic/ferritic :180 80-250 m/min
K 16 Grey cast iron (GG) Pearlitic/martensiti :260 130-240 m/min
K 17 Nodular cast iron (GGG) Ferritic :160 150-270 m/min
K 18 Nodular cast iron (GGG) Pearlitic :250 150-270 m/min
K 19 Malleable cast iron Ferritic :130 150-270 m/min
K 20 Malleable cast iron Pearlitic :230 140-240 m/min
S 31 High temp. alloys Fe based Annealed :200 20-40 m/min
S 32 High temp. alloys Fe based Cured :280 20-30 m/min
S 33 High temp. alloys. Ni or Co based Annealed :250 20-30 m/min
S 34 High temp. alloys. Ni or Co based Cured :350 20-30 m/min
S 35 High temp. alloys. Ni or Co based Castr :320 20-30 m/min
S 36 Titanium (pure) Pure :310 30-80 m/min
S 37 Titanium Ti alloys Alpha+beta alloys cu :310 30-80 m/min