ISCAR 16 ERM AG 55 IC908 Insert

Grade : IC908

ISCAR 16 ERM AG 55 IC908 Insert. A hard, fine grain substrate with excellent chipping resistance, combined with a TiAlN PVD coating. Provides high wear and oxidation resistance. Recommended for a very wide range of materials applications and machining conditions.

ISO Range – P/M/K(P15-P30)(M20-M30)(K20-K30)
ISO Range – H/S/N(H20-H30)(S10-S25)

 

Grade or Coating TypePVD
Coating LayersTiAlN

Cutting Speed for:

16ERM AG 55 IC908 – 5921213

ISOMaterialMaterial DescriptionMaterial ConditionCutting Speed Recommendations
P1Non-alloy steel and cast steel, free cutting steel <0.25%CAnnealed :12587-166 m/min
P2Non-alloy steel and cast steel, free cutting steel >=0.25%CAnnealed :19084-160 m/min
P3Non-alloy steel and cast steel, free cutting steel <0.55%CQuench and tempered. :25080-155 m/min
P4Non-alloy steel and cast steel, free cutting steel >=0.55%CAnnealed :22078-149 m/min
P5Non-alloy steel and cast steel, free cutting steel >=0.55%CQuenched & tempered. :30077-142 m/min
P6Low alloy & cast steel (less than 5% of alloying elements)Annealed :20092-140 m/min
P7Low alloy & cast steel (less than 5% of alloying elements)Quenched & tempered :27585-128 m/min
P8Low alloy & cast steel (less than 5% of alloying elements)Quenched & tempered :30080-123 m/min
P9Low alloy & cast steel (less than 5% of alloying elements)Quenched & tempered :35074-119 m/min
P10High alloyed steel, cast steel and tool steelAnnealed :20072-124 m/min
P11High alloyed steel, cast steel and tool steelQuenched & tempered :32560-110 m/min
P12Stainless steel and cast steelFerritic/martensitic :20086-130 m/min
P13Stainless steel and cast steelMartensitic :24085-122 m/min
M14Stainless steel and cast steelAustenitic :18078-122 m/min
K15Grey cast iron (GG)Pearlitic/ferritic :18067-118 m/min
K16Grey cast iron (GG)Pearlitic/martensiti :26060-100 m/min
K17Nodular cast iron (GGG)Ferritic :16056-112 m/min
K18Nodular cast iron (GGG)Pearlitic :25052-95 m/min
K19Malleable cast ironFerritic :13054-100 m/min
K20Malleable cast ironPearlitic :23052-109 m/min
N21Aluminum-wrought alloyNot cureable : 6084-257 m/min
N22Aluminum-wrought alloyCured :10080-204 m/min
N23Aluminum-cast, alloyed <12% SiNot cureable : 75118-300 m/min
N24Aluminum-cast, alloyedCured : 90118-246 m/min
N25Aluminum-cast, alloyed >12% SiHigh temperature :13098-226 m/min
N26Copper alloys >1% PbFree cutting :11094-271 m/min
N27Copper alloysBrass : 9094-271 m/min
N28Copper alloysElectrolitic copper :10094-271 m/min
N29Non metallicDuro& fiber plastics : 6072-278 m/min
N30Non metallicHard rubber : 5568-262 m/min
S31High temp. alloys Fe basedAnnealed :20025-52 m/min
S32High temp. alloys Fe basedCured :28023-46 m/min
S33High temp. alloys. Ni or Co basedAnnealed :25020-34 m/min
S34High temp. alloys. Ni or Co basedCured :35015-29 m/min
S35High temp. alloys. Ni or Co basedCastr :32017-31 m/min
S36Titanium (pure)Pure :31048-86 m/min
S37Titanium Ti alloysAlpha+beta alloys cu :31026-58 m/min
H38Hardened steelHardened :56032-60 m/min
H39Hardened steelHardened :65429-47 m/min
H40Chilled cast ironCast :40032-60 m/min
H41Cast ironHardened :56029-54 m/min